Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.68 GPa | 824 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP JF003E PES LNP* THERMOCOMP* JF003E is a compound based on Polyethersulfone resin containing 15% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 5.68 GPa | 824 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON NV003E PC+ABS (Asia Pacific) LNP* Verton* NV003E is a compound based on PC+ABS Blend resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 5.68 GPa | 824 ksi | ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX870 PPE+PA6 (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.68 GPa | 824 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX870 PPE+PA6 (Asia Pacific) |
|||
Flexural Modulus | 5.68 GPa | 824 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX870 PPE+PA6 (Asia Pacific) |
|||
Flexural Modulus | 5.68 GPa | 824 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON NV003E PC+ABS LNP* VERTON* NV003E is a compound based on PC+ABS Blend resin containing 15% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |
|||
Flexural Modulus | 5.68 GPa | 824 ksi | ASTM D790 |
Teknor Apex Sinpolene GPP1630 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 30% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |