Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.65 GPa | 819 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY DF2049 PC (Asia Pacific) LNP* Lubriloy* DF2049 is a compound based on Polycarbonate resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
Flexural Modulus | 5.65 GPa | 819 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX06411 PC LNP* THERMOCOMP* DX06411 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |
|||
Flexural Modulus | 5.65 GPa | 819 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX06411 PC (Asia Pacific) LNP* Thermocomp* DX06411 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Flexural Modulus | 5.65 GPa | 819 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp JF003L PES LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r.. |
|||
Flexural Modulus | 5.65 GPa | 819 ksi | ISO 178 |
Polyplastics Duranex® C5315 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |