Polymer Property : Flexural Modulus = 8.91 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.91 GPa
1290 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL36EU PC
LNP* Lubricomp* DFL36EU is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Easy Molding and UV Stabilized.
Flexural Modulus 8.91 GPa
1290 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ507 PBT+PC
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Flexural Modulus 8.91 GPa
1290 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Flexural Modulus 8.91 GPa
1290 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Flexural Modulus 8.91 GPa
1290 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES
LNP* THERMOCOMP* JF006E is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 8.91 GPa
1290 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 8.91 GPa
1290 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp XF006S
LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region..
Flexural Modulus 8.91 GPa
1290 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP XF006S PA
LNP* THERMOCOMP* XF006S is a compound based on Amorphous Nylon containing 30% Glass Fiber. Added feature of th is grade is: Heat Stabilized.
Flexural Modulus 8.91 GPa
1290 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP JF006EXZ PES
LNP* THERMOCOMP* JF006EXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.