Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.69 GPa | 1260 ksi | ASTM D790 |
Plenco 51335 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51335 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in black only.Information .. |
|||
Flexural Modulus | 8.69 GPa | 1260 ksi | ASTM D790 |
Polymer Resources AC-G25 Acetal Copolymer, 25% Glass Reinforced Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 8.69 GPa | 1260 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF30 FR-N 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Halogen FreeInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 8.69 GPa | 1260 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6,6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricatedFeatures: LubricatedProcessing Method: Injection MoldingAppearance: .. |
|||
Flexural Modulus | 8.69 GPa | 1260 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing. |