Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.55 GPa | 1240 ksi | ASTM D790 |
PolyOne Stat-Tech™ PC-15CF/000 Black Polycarbonate (PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Modulus | 8.55 GPa | 1240 ksi | ASTM D790 |
Techmer ES HiFill® PVDF CF15 BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 8.55 GPa | 1240 ksi | ASTM D790 |
Techmer ES HiFill® PVDF CF15-M BK 15% Milled Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Carbon Fiber, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 8.55 GPa | 1240 ksi | ISO 178 |
Polyram PlusTek PA7800G33 Nylon 6.6 for Injection Molding, 33% Glass Fiber Reinforced, Heat Stabilized, Impact Modified 33% Glass fiber reinforced, heat stabilized, impact modified Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 8.55 GPa | 1240 ksi | ASTM D790 |
Westlake Plastics Kynar® PVDF CN-F Polyvinylidene Fluoride (conductive) Non-sloughing carbon-fiber-filled material with resistance to most chemicals and solvents mechanically strong and tough, thermally stable to 335F, flame and abrasion resistant, and easily fabricated.. |
|||
Flexural Modulus | 8.55 GPa | 1240 ksi | ASTM D790 |
Adell HR-36 30% Glass Reinforced Heat Stabilized PBT |
|||
Flexural Modulus | 8.55 GPa | 1240 ksi | ISO 178 |
BASF Ultramid® A3EG6 BK 00564 PA66 (Dry) Information provided by BASF |