Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.28 GPa | 1200 ksi | ASTM D790 |
PlastiComp Complet® LGF30-PA66 MT 30% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Flexural Modulus | 8.28 GPa | 1200 ksi | ISO 178 |
Azdel AZMET® CM20350 35% continuous random fiber mat / PBT resin matrix AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polybutylene Terephthalate (PBT) resin matrix. This composite material fea.. |
|||
Flexural Modulus | 8.28 GPa | 1200 ksi | ASTM Test |
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6. |
|||
Flexural Modulus | 8.28 GPa | 1200 ksi | ASTM Test |
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Dry) Ultramid 1503-2 NF2004 is a 33% glass reinforced, heat stabilized injection molding PA6/6. |