Mechanical Properties Metric English Comments
Flexural Modulus 5.45 GPa
790 ksi
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Flexural Modulus 5.45 GPa
790 ksi
Tangent; ASTM D790
RheTech Products F25-01 34% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Support ductsHousingsBattery traysArm rest insertsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 5.45 GPa
790 ksi
Tangent; ASTM D790
RheTech Products F35-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Interior trimUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 5.45 GPa
790 ksi
after 16 hours in 50°C water
Malvern Minerals Thermoplastic Polyester with Novacite® 1250 Quartz Filler
Product data demonstrates the effect of the Novacite (untreated lamellar quartz) filler. A separate entry demonstrates the effect of surface-treated Novakup filler in thermoplastic polyester Th..
Flexural Modulus 5.45 GPa
790 ksi
ASTM D790
Techmer ES Electrablend® PA6/6 GF13 SS10 BK 13/10% Glass/Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Stainless Steel Reinforcement, 13/10% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation..
Flexural Modulus 5.45 GPa
790 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT
LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity.
Flexural Modulus 5.45 GPa
790 ksi
Tangent; ASTM D790
Plastics Group Polifil® GFPPCC-30 30% Glass Reinforced Polypropylene
Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature..
Flexural Modulus 5.45 GPa
790 ksi
ASTM D790
Chesterton ARC S2 Ceramic reinforced erosion resistant coating
Description: An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% soli..
Flexural Modulus 5.45 GPa
790 ksi
ASTM D790
Chesterton MRS S2 Metal Rebuilding System
An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% solids. MRS S2 is..
Flexural Modulus 5.45 GPa
790 ksi
ASTM D790, ISO 178
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber
Characteristics: 17% glass fibre filled
Flexural Modulus 5.45 GPa
790 ksi
ASTM D790
Asahi Kasei Thermylene® P7-30FG-0684 30% Glass Fiber Reinforced, Heat and UV Stabilized
Information provided by Asahi Thermofil