Mechanical Properties Metric English Comments
Flexural Modulus >= 0.550 GPa
>= 79.8 ksi
ASTM D1238
NIZHNEKAMSKNEFTEKHIM PE 4026Z (26460) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Flexural Modulus >= 0.550 GPa
>= 79.8 ksi
ASTM D790
NIZHNEKAMSKNEFTEKHIM PE 4028X (28435) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Flexural Modulus 0.550 GPa
79.8 ksi
Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790
Phillips Sumika Marlex® ABF-080 Thermoplastic Polyolefin  (discontinued **)
Applications: Air damInterior trimInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued prior t..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
3M Dyneon™ PFA X 6505 UHP Perfluoroalkoxy Fluorothermoplastic  (discontinued **)
Dyneon PFA X 6502 UPH, PFA X 6505 UHP and PFA X 6515 UHP are ultra-high purity fluorothermoplastics. These resins were developed for high-purity applications requiring ultra-low levels of metal and ..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
3M Dyneon™ PFA 6502N Perfluoroalkoxy Fluorothermoplastic  (discontinued **)
The excellent chemical temperature resistance of Dyneon™ 6500N PFA is available across a range of melt flow indices, for optimal processability. Dyneon™ PFA 6502N, the highest molecular weight gra..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
3M Dyneon™ PFA 6505N Perfluoroalkoxy Fluorothermoplastic  (discontinued **)
The excellent chemical temperature resistance of Dyneon™ 6500N PFA is available across a range of melt flow indices, for optimal processability. Dyneon™ PFA 6502N, the highest molecular weight gra..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
3M Dyneon™ PFA 6502TA Perfluoroalkoxy Fluorothermoplastic  (discontinued **)
Dyneon PFA 6502TA is a fluorothermoplastic resin developed for compression molding applications. PFA 6502TA has a wide processing window with excellent color stability when longer residence times or..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
3M Dyneon™ PFA 6503 A EPC Perfluoroalkoxy Fluorothermoplastic  (discontinued **)
Dyneon PFA 6503 A EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick ..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
3M Dyneon™ PFA 6503 C EPC Perfluoroalkoxy Fluorothermoplastic  (discontinued **)
Dyneon PFA 6503 C EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick ..
Flexural Modulus 0.550 GPa
79.8 ksi
2mm/min; ASTM D790-86
Micropol Microcene MC121 Metallocene Based Polyethylene Rotational Molding Powder
Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. ..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D760-66
Micropol Microlin ML91 Linear Polyethylene Rotational Molding Powder
Information provided by Micropol Limited
Flexural Modulus 0.550 GPa
79.8 ksi
Tangent at 0.05 in/min; ASTM D790A
LyondellBasell Hifaxâ„¢ ETA-3081 Thermoplastic Olefin Resin
Key Features: medium high melt flow, medium modulus, paintable thermoplastic olefin resin, excellent balance of properties, excellent processability, good paintability and paint durability, good sur..
Flexural Modulus 0.550 GPa
79.8 ksi
ISO 178
LyondellBasell Hifaxâ„¢ ETA-3104HF Thermoplastic Olefin Resin
Key Features: medium melt flow, medium modulus thermoplastic elastomeric olefin resin, good impact and stiffness balance, good dimensional stability, good processabilityApplications: molded-in color..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
Sumitomo Chemical ESPOLEX® 903 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Flexural Modulus 0.550 GPa
79.8 ksi
50% humidity; ISO 178
Borealis Bormed™ SC820CF Polypropylene Random Copolymer
Bormed™ SC820CF is a very soft random heterophasic copolymer. Applications: Bormed™ SC820CF is recommended for packaging for medical devices. Bormed™ SC820CF contains no slip, antiblock, antist..
Flexural Modulus 0.550 GPa
79.8 ksi
ISO 178
Borealis Borseal™ RE939CF Polypropylene Copolymer
Borseal™ RE939CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: Borseal™ RE939CF is designed for: Food packaging,..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
Tipco Tipcolene® TPE-HMI TPE HMI - Impact Modified Polypropylene Copolymer Compound with High Flow, Soft Touch
High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Modulus 0.550 GPa
79.8 ksi
50%RH; ISO 178
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..
Flexural Modulus 0.550 GPa
79.8 ksi
SAE J949
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (7 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
3M Dyneon™ PFA 6502 TAZ Perfluoroalkoxy Fluorothermoplastic Granules
3M™ Dyneon™ PFA 6502TAZ is a fluorothermoplastic resin for compression molding applications. PFA 6502TAZ has a wide processing window with excellent color stability when longer residence times or ..
Flexural Modulus 0.550 GPa
79.8 ksi
3M Dyneon™ PFA 6502 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules
Dyneon PFA X 6502 UPH, PFA X 6505 UHP and PFA X 6515 UHP are a new series of ultra-high purity fluorothermoplastics. These resins were developed for high-purity applications requiring ultra-low leve..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
3M Dyneon™ PFA 6502TZ Perfluoroalkoxy Fluorothermoplastic Granules
3M™ Dyneon™ PFA 6502TZ is a fluorothermoplastic resin for transfer molding applications and extrusion of claddings and linings. Dyneon PFA 6502TZ allows for easy processing under low shear rates, ..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
3M Dyneon™ PFA 6503PAZ Fluoroplastic Powder
3M™ Dyneon™ Fluoroplastic Powder PFA 6503PAZ is a fluorothermoplastic powder designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tan..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
3M Dyneon™ PFA 6503PBZ Fluoroplastic Powder
3M™ Dyneon™ Fluoroplastic Powder PFA 6503PBZ is a fluorothermoplastic powder with excellent thermal stability characteristics, designed for use in thin film powder coatings. Typical applications i..
Flexural Modulus 0.550 GPa
79.8 ksi
Injection Molded Bars (0.5"x.125"x 5"); ASTM D790
3M Dyneon™ PFA 6505TZ Fluoroplastic Granules
3M™ Dyneon™ Fluoroplastic Granules PFA 6505TZ (a fully fluorinated copolymer of tetrafluoroethylene and perfluorovinylether) has exceptional temperature resistance, excellent electrical properties..
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
3M Dyneon™ PFA 6503 B EPC Perfluoroalkoxy Fluorothermoplastic  (discontinued **)
Dyneon PFA 6503 B EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick ..
Flexural Modulus 0.550 - 2.28 GPa
79.8 - 331 ksi
Average value: 1.38 GPa Grade Count:141