Polymer Property : Flexural Modulus = 77.9 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.45 - 77.9 GPa
500 - 11300 ksi
Average value: 16.1 GPa Grade Count:26
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..