Polymer Property : Flexural Modulus = 760 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.24 GPa
760 ksi
Tangent; ASTM D790
RheTech Products GC30P105-08FA 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black
Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 5.24 GPa
760 ksi
ASTM D790
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced
Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Flexural Modulus 5.24 GPa
760 ksi
ASTM Data
BASF Capron® HPN 9333G Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron HPN 9333G is a 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface a..
Flexural Modulus 5.24 GPa
760 ksi
Fibre Glast 1110 L Vinyl Ester Resin (Laminate Properties)
#1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resista..
Flexural Modulus 5.24 GPa
760 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2110 PEI (Asia Pacific)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 5.24 GPa
760 ksi
ASTM D790
Techmer ES HiFill® PEI/C GF10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc.
Flexural Modulus 5.24 GPa
760 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RZ006S PA 66
LNP* THERMOCOMP* RZ006S is a compound based on Nylon 66 resin containing 30% Milled Glass. Added feature of this material is: Heat Stabilized.
Flexural Modulus 5.24 GPa
760 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RZ006S PA 66 (Asia Pacific)
LNP* Thermocomp* RZ006S is a compound based on Nylon 66 resin containing Milled Glass.
Flexural Modulus 5.24 GPa
760 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL PX4605 PPE+PS
PPE+PS blend. 20% Glass reinforced. High heat. Dimensional stability. Suitable for automotive and E/E applications.
Flexural Modulus 5.24 GPa
760 ksi
2.6 mm/min, 100 mm span; ASTM D 790
SABIC Innovative Plastics Ultem 2110N PEI (Asia Pacific)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 5.24 GPa
760 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2110R PEI
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 5.24 GPa
760 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2110R PEI (Asia Pacific)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 5.24 GPa
760 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Ultem ATX102R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 5.24 GPa
760 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 5.24 GPa
760 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region..
Flexural Modulus 5.24 GPa
760 ksi
ASTM D790
Ecomass® 1080CO94 Copper Powder Filled Polyamide Alloy, Injection Molding
Moderate Specific Gravity, Copper Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing..
Flexural Modulus 5.24 GPa
760 ksi
ASTM D790
Aaron Industries AAROPRENE® MFN 6001 Mineral Filled Nylon 6
AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified.
Flexural Modulus 5.24 GPa
760 ksi
ASTM D790
Aaron Industries AAROPRENE® GFPC 5020 Glass Filled Polycarbonate
AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Flexural Modulus 5.24 GPa
760 ksi
ASTM D790
Techmer ES Plastiblend® ABS/PBT GF15
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Modulus 5.24 GPa
760 ksi
ASTM Data
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with..
Flexural Modulus 5.24 GPa
760 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2110 PEI
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 5.24 GPa
760 ksi
2.6 mm/min, 100 mm span; ASTM D 790
SABIC Innovative Plastics Ultem 2110N PEI
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 5.24 GPa
760 ksi
ASTM D790
Techmer ES HiFill FR® PPO/HIPS GF20 BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by Weight Appearance: BlackInformation provided by TP Composites, Inc.