Polymer Property : Flexural Modulus = 721 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.97 GPa
721 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® MC5215 PC+ABS
Flexural Modulus 4.97 GPa
721 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® MC5215 PC+ABS (Asia Pacific)