Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.84 GPa | 1140 ksi | ASTM D790 |
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Flexural Modulus | 7.84 GPa | 1140 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea.. |
|||
Flexural Modulus | 7.84 GPa | 1140 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific) LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System. |