Polymer Property : Flexural Modulus = 7.40 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0510 GPa
7.40 ksi
ASTM D790
Toyobo PELPRENE™ P40H Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
Flexural Modulus 0.0510 GPa
7.40 ksi
ASTM D790
Toyobo PELPRENE™ P40H-05 Polyester TPE, Non-smell, Non-deposit
Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo.
Flexural Modulus 0.0510 GPa
7.40 ksi
ASTM D790
Toyobo PELPRENE™ P40U Polyester TPE, Weather-resistant
Features: Polyester TPE, Weather-resistantInformation provided by Toyobo.
Flexural Modulus 0.0510 GPa
7.40 ksi
1% Secant, ASTM D790
ExxonMobil Escorene® LD-728 High EVA Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams..