Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.31 GPa | 1060 ksi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® PC-30GF/000 BLACK Polycarbonate (PC) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 7.31 GPa @Temperature 150 °C |
1060 ksi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Flexural Modulus | 7.31 GPa | 1060 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF27 SL2 27% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 27% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Flexural Modulus | 7.31 GPa | 1060 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN133TL (Dry) Nylon 66, 33% Glass Fiber Reinforced, Lubricated, Impact Modified Features: Impact modifiedLubricatedGood toughnessForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 7.31 GPa | 1060 ksi | Tangent; ASTM D790 |
Washington Penn High Modulus Polypropylene Homopolymer 40% Glass Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Flexural Modulus | 7.31 GPa | 1060 ksi | Tangent; ASTM D790 |
Washington Penn Homopolymer Polypropylene 40% Glass Reinforced Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Flexural Modulus | 7.31 GPa | 1060 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-40FG-0874 40% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 7.31 GPa | 1060 ksi | ASTM D790 |
Asahi Kasei Thermylene® P7-40FG-0790 40% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 7.31 GPa | 1060 ksi | ASTM Value |
BASF Capron® 8232G HS BK-102 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8232G HS BK-102 is a pigmented black, heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional.. |
|||
Flexural Modulus | 7.31 GPa @Temperature 150 °C |
1060 ksi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |