Mechanical Properties Metric English Comments
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC (Asia Pacific)
LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC
LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP KFL32R Acetal Copolymer
LNP LUBRICOMP* KFL32R is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE. Added feature of this material is: Easy Release, Wear Resistant.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP (Asia Pacific)
LNP* LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing PTFE, Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66
LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific)
LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Flexural Modulus 4.82 GPa
699 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® 855 PBT
15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts.
Flexural Modulus 4.82 GPa
699 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® 855 PBT (Asia Pacific)
15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts.
Flexural Modulus 4.82 GPa
699 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® DR51 PBT
15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors
Flexural Modulus 4.82 GPa
699 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® DR51 PBT (Asia Pacific)
15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors
Flexural Modulus 4.82 GPa
699 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific)
15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia ..
Flexural Modulus 4.82 GPa
699 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East)
15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp EB004 PEI
LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp EB004 PEI (Asia Pacific)
LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 (Asia Pacific)
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly
LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific)
LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible.
Flexural Modulus 4.82 GPa
699 ksi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 5201-12 Polycarbonate Resin
Overview: CALIBREâ„¢ 5201-12 polycarbonate resin is 20% glass reinforced containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. CALI..
Flexural Modulus 4.82 GPa
699 ksi
3-point; ISO 178
Styron CALIBREâ„¢ 5201-8 Polycarbonate Resin
Overview: CALIBREâ„¢ 5201-8 polycarbonate resin is 20% glass reinforced containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. CALIB..
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 4.82 GPa
699 ksi
ASTM D790
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 4.82 GPa
699 ksi
1.3 mm/min, 50 mm span; ASTM D790