Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.60 GPa @Temperature 23.0 °C |
667 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A33^E F15 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® BFL2015 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by .. |
|||
Flexural Modulus | 4.60 GPa @Temperature 175 °C |
667 ksi @Temperature 347 °F |
Conditioned; ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ISO 178 |
Nilit FRIANYL A63 KV35 Nylon 6.6 for injection molding, 35% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ASTM D790 |
Kostat G148BK TAB Spacer Reels KOSTATs TAB Spacer Reels are ideal for shipment and storage of any components packaged in TAB spacer tapes. KOSTATSs TAB Spacer Reels, uniquely formulated and manufactured with the most advanced in.. |
|||
Flexural Modulus | 4.60 GPa @Temperature 175 °C |
667 ksi @Temperature 347 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12 LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP ZX08005 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZX08005 is a Compound based on PPE + PS Blend resin, containing Mineral. Added features include: Improved Dielectric Properties. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX92002 PC (Europe-Africa-Middle East) LNP* Stat-kon* DX92002 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 9X02841 PBT+PC LNP* Thermocmop* 9X02841 is a PBT/Polycarbonate blend containing proprietary fillers. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MF0044E PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF0044E is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features include: Non-Halogen Flame Retardant, Easy Molding.This data was supplied .. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WFB33E PBT (Europe-Africa-Middle East) LNP *THERMOCOMP* WFB33E is a compound based on Polybutylene Terephalate resin containing Glass Fiber and Glass Bead. Added features include Easy Molding. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ISO 178 |
Unitika TERRAMAC TE-7000 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ISO 178 |
Polyram PlusTek PB300G2 Nylon 6 for Injection Molding, 10% Glass-Fiber Reinforced 10% Glass-fiber reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 570 NC000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler for injection molding. Delrin 570 has very high stiff.. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ASTM D790 |
E-Polymers TEKANATE™ G715FR , Flame Retardant, 15% Glass Fiber Reinforced Poly Carbonate 15% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 4.60 GPa @Temperature 23.0 °C |
667 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Delrin® FG570 NC000 Acetal Homopolymer Delrin® FG570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber for injection molding. It has high stiffness and low warpage. It has been developed for consideration in appl.. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 412 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ASTM D790 |
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL329 PC LNP LUBRICOMP* DFL329 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Flexural Modulus | 4.60 GPa | 667 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH327G28 Polypropylene Homopolymer, 28% Glass Filled SAXALEN PPH327G28 is a 28% glass filled Polypropylene - Homopolymer injection molding grade with increased stiffness.Information provided by SAX Polymers |