Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.59 GPa | 666 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Flexural Modulus | 4.59 GPa | 666 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Faradex ES003DE PEI LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 4.59 GPa | 666 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP FARADEX ES003E PEI LNP* FARADEX* ES003E is a Polyetherimide resin containing 15% Stainless Steel Fibers. Added feature of this grade is: EMI/RFI Shielding. |
|||
Flexural Modulus | 4.59 GPa | 666 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Flexural Modulus | 4.59 GPa | 666 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Flexural Modulus | 4.59 GPa | 666 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP IF003 PA 6/12 LNP THERMOCOMP* IF003 is a compound based on Nylon 6/12 resin containing 15% Glass Fiber. |