Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.430 GPa | 62.4 ksi | ASTM D790 |
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Flexural Modulus | 0.430 GPa @Temperature 90.0 °C |
62.4 ksi @Temperature 194 °F |
ASTM D790 |
LATI LATAN 3E71 Polyoxymethylene Copolymer (POM) with Elastomer
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Flexural Modulus | 0.430 GPa | 62.4 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 301 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.430 GPa | 62.4 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 301 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.430 GPa | 62.4 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 301 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.430 GPa | 62.4 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 301 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.430 GPa | 62.4 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 301 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.430 GPa | 62.4 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 301 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.430 GPa | 62.4 ksi | SAE J949 |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (7 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |