Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.420 GPa | 60.9 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 110-1328 LMDPE Rotational Molding Resin Description: ICORENE 110-1328 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po.. |
|||
Flexural Modulus | 0.420 GPa | 60.9 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 115-1323 LMDPE Rotational Molding Resin Description: ICORENE 115-1323 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Flexural Modulus | 0.420 GPa | 60.9 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 190-1323 LMDPE Rotational Molding Resin Description: ICORENE 190-1323 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key.. |
|||
Flexural Modulus | 0.420 GPa | 60.9 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 190-1328 LMDPE Rotational Molding Resin Description: ICORENE 190-1328 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key.. |
|||
Flexural Modulus | 0.420 GPa | 60.9 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 324-1323 LMDPE Rotational Molding Resin Description: ICORENE 324-1323 is a linear medium density polyethylene developed for use in rotational molding. It has very good flow properties allowing the material to reproduce fine detail and me.. |
|||
Flexural Modulus | 0.420 GPa | 60.9 ksi | ASTM D790 |
Sumitomo Chemical ESPOLEX® WT521 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Flexural Modulus | 0.420 GPa | 60.9 ksi | SAE J949 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.420 GPa | 60.9 ksi | ASTM D790 |
DuPont™ Surlyn® 7940 Ionomer Resin, Lithium Surlyn® 7940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne.. |