Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 6.83 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.83 GPa
991 ksi
ASTM D790
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h..
Flexural Modulus 6.83 GPa

@Temperature 100 °C
991 ksi

@Temperature 212 °F
ISO 178
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Flexural Modulus 6.83 GPa
990 ksi
ASTM D790
Techmer ES Electrablend® PA6/6 C10 BK 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightFeatures: ConductiveAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 6.83 GPa
991 ksi
ASTM D790
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
Torlon® 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon® PAI h..
Flexural Modulus 6.83 GPa
990 ksi
ASTM D790
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass
Information provided by Star Plastics, Inc.
Flexural Modulus 6.83 GPa
990 ksi
ASTM D790
Techmer ES Luriblend® PA6/6 CF10 TL15 BK 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceAppearance: Blac..
Flexural Modulus 6.83 GPa
990 ksi
ASTM D790
Chesterton ARC 858 Abrasion resistant rebuilding and faring composite
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 0.15 mm (60 mils) or m..
Flexural Modulus 6.83 GPa
990 ksi
ASTM D790
Chesterton MRS 58 Metal Rebuilding System
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 1.5 mm (60 mils) or mo..
Flexural Modulus 6.83 GPa

@Temperature 100 °C
991 ksi

@Temperature 212 °F
ISO 178
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..
Copyright © lookpolymers.com All Rights Reserved