Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.621 GPa | 960.3 ksi | ASTM D-790 |
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% long glass fiber reinforcementInformation provided by PlastiCom.. |