Polymer Property : Flexural Modulus = 6.32 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.32 GPa
917 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN
LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A..
Flexural Modulus 6.32 GPa
917 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL34EH PC
LNP* LUBRICOMP* DFL34EH is a compound based on Polycarbonate containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Easy Molding, Healthcare, Wear Resistant.
Flexural Modulus 6.32 GPa
917 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON DEL329E PC (Asia Pacific)
LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, ..
Flexural Modulus 6.32 GPa
917 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS
LNP* THERMOCOMP* CX05470 is a compound based on Polystyrene resin containing 20% Glass Fiber.