Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.06 GPa | 879 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A.. |
|||
Flexural Modulus | 6.06 GPa | 879 ksi | ASTM D790 |
Plenco 50015 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu.. |
|||
Flexural Modulus | 6.06 GPa | 879 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WF0039U PBT LNP* THERMOCOMP* WF0039U is a compound based on PBT resin containing 15% Glass Fiber. Added features of this grade include: Flame Retardant and UV Stabilized. |