Polymer Property : Flexural Modulus = 555 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.83 GPa
555 ksi
ASTM D790
NatureWorks® Ingeo™ 2003D General Purpose Transparent Extrusion Grade Biopolymer
NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed fo..
Flexural Modulus 3.82 GPa

@Thickness 3.20 mm
555 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical Lupox® HI2100M PBT+GF10%
Description: Injection Molding, PBT+GF10%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 65997-17-3, 155123-66-3 and 30965-26-5Information provided by LG Chemical
Flexural Modulus 3.82 GPa

@Thickness 6.40 mm
555 ksi

@Thickness 0.252 in
5mm/min; ASTM D790
LG Chemical Lupox® TE5100 PBT+PC+GF10%
Description: Injection Molding, PBT+PC+GF10%, High Impact resistant, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 30965-26-5, 103598-77-2 and 65997-17-3Information provided..
Flexural Modulus 3.83 GPa
555 ksi
ASTM D790
PlastxWorld CEVIAN® S1210 PC/ABS alloy
Glass fiber reinforced PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Modulus 3.83 GPa
555 ksi
ASTM D790
PlastxWorld CEVIAN® VGR10 10% GF ABS
Glass fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.