Polymer Property : Flexural Modulus = 5.899 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.899 GPa
855.6 ksi
ASTM D790
Aclo Accutech Polycarbonate POL050G20L Glass Reinforced
Flexural Modulus 5.899 GPa
855.6 ksi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0336M40CL Mica Reinforced Coupled