Polymer Property : Flexural Modulus = 5.85 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.85 GPa
848 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific)
LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.This data was suppli..
Flexural Modulus 5.85 GPa
848 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Flexural Modulus 5.85 GPa
848 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Flexural Modulus 5.85 GPa
848 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Flexural Modulus 5.85 GPa
848 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Flexural Modulus 5.85 GPa
848 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Flexural Modulus 5.85 GPa
848 ksi
ISO 178
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Flexural Modulus 5.85 GPa
848 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness..
Flexural Modulus 5.85 GPa

@Temperature 60.0 °C
848 ksi

@Temperature 140 °F
ASTM D790
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Flexural Modulus 5.85 GPa
848 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HFD4412 PC
Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Flexural Modulus 5.85 GPa
848 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HFD4412 PC (Europe-Africa-Middle East)
Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Flexural Modulus 5.85 GPa
848 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HFD4412 PC (Asia Pacific)
Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.