Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.74 GPa | 833 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable. |