Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.72 GPa | 830 ksi | ASTM D790 |
PolyOne Gravi-Tech™ GRV-NY-030-SS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Flexural Modulus | 5.72 GPa | 830 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 and 5VA listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Flexural Modulus | 5.72 GPa | 830 ksi | ASTM D790 |
Techmer ES HiFill® PA6 CM40 HS 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural .. |
|||
Flexural Modulus | 5.72 GPa | 830 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF40 L 40% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Comp.. |
|||
Flexural Modulus | 5.72 GPa | 830 ksi | ASTM D790 |
Techmer ES Plaslube® J-80/20/TF/15 NAT Acetal (POM) Copolymer |
|||
Flexural Modulus | 5.72 GPa | 830 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP IF004 PA6.12 LNP* THERMOCOMP* IF004 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 5.72 GPa | 830 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL IGN320 PPE+PS 20% glass reinforced PPE + PS. High heat, high modulus automotive applications like ignition coils. |
|||
Flexural Modulus | 5.72 GPa | 830 ksi | ASTM D790 |
Techmer ES Plaslube® J-80/20/TF/15 BK223 Acetal (POM) Copolymer |
|||
Flexural Modulus | 5.72 GPa | 830 ksi | ASTM D790 |
Clariant PA123G25 Nylon 66, 25% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 5.72 GPa | 830 ksi | ASTM D790 |
Clariant Renol PPSP0006HW Polypropylene Homopolymer, Heavy Weight Compound Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 5.72 GPa | 830 ksi | ASTM D790 |
Asahi Kasei Thermylene® P7-30FG-0890 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |