Mechanical Properties Metric English Comments
Flexural Modulus 5.69 GPa
825 ksi
Tangent; ASTM D790
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 5.69 GPa
825 ksi
ASTM D790
Oxford Polymers 20GF 20% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding
20% Glass Fiber Filled Polyetherimide for Extrusion and Injection MoldingInformation provided by Oxford Polymers.
Flexural Modulus 5.69 GPa
825 ksi
ASTM D790
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced
Acrylonitrile Butadiene Styrene, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Flexural Modulus 5.69 GPa

@Thickness 3.20 mm
825 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMAX GP5200B PBT+ABS+GF20%
Description: Injection Molding Grade, PBT+ABS+GF20%, General PurposeApplication: E&E (Speaker Frame)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 9003-54-7Information provided by LG Chemical
Flexural Modulus 5.69 GPa

@Thickness 3.20 mm
825 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical Lupox® SG5200 PBT+PET+GF20%
Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical
Flexural Modulus 5.69 GPa
825 ksi
ASTM D790
Kotec Carbotex KG-20MRA Polycarbonate, 20% Glass Fiber Reinforced
Features: Glass fiber 20% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E ..
Flexural Modulus 5.69 GPa
825 ksi
ASTM D790
Kotec Carbotex KGN-20MRA Polycarbonate, Flame Retardant, 20% Glass Fiber Reinforced
Features: Glass fiber 20% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E ..
Flexural Modulus 5.69 GPa

@Thickness 3.20 mm
825 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance
Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG..
Flexural Modulus 5.69 GPa
825 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN133G20 G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 5.69 GPa

@Thickness 3.20 mm
825 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical Lupox® GP2156FM PBT+GF15%
Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
Flexural Modulus 5.69 GPa
825 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DEL22P PC
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Electrically Conductive. Exceptional Processing, Wear..
Flexural Modulus 5.69 GPa
825 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® VG-4920F ABS, Glass Filled FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 5.69 GPa
825 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® VG-4920F ABS, Glass Filled FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 5.69 GPa
825 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DEL22P PC (Asia Pacific)
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 5.69 GPa
825 ksi
ASTM D790
Techmer ES Electrablend® PA6/6 03005 CF Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact..
Flexural Modulus 5.69 GPa
825 ksi
ASTM D790
PlastxWorld CEVIAN® B5723 15% GF PBT/ABS Alloy
Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc.
Flexural Modulus 5.69 GPa
825 ksi
Tangent; ASTM D790
Washington Penn High Modulus Polypropylene Homopolymer 40% Mica Filled
Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a..