Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.80 - 5.50 GPa @Temperature 90.0 - 90.0 °C |
696 - 798 ksi @Temperature 194 - 194 °F |
Average value: 5.15 GPa Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Flexural Modulus | 0.200 - 5.50 GPa | 29.0 - 798 ksi | Average value: 2.20 GPa Grade Count:88 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Flexural Modulus | 5.00 - 5.50 GPa | 725 - 798 ksi | ASTM D790 |
Loxim 830 01 HBCC Polypropylene Compound 30% Chemically Coupled, Flame Retardant Information provided by Loxim Industries |
|||
Flexural Modulus | 0.305 - 5.50 GPa @Temperature -40.0 - 120 °C |
44.2 - 798 ksi @Temperature -40.0 - 248 °F |
Average value: 1.40 GPa Grade Count:8 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |