Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.445 GPa | 499.7 ksi | chs 0.05 in/min; tangent; ASTM D790 |
Diamond Polymers SAN 330 BEADS Styrene Acrylonitrile, Transparent Engineering Thermoplastic, High Flow Natural Beads Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |