Mechanical Properties Metric English Comments
Flexural Modulus 3.037 GPa
440.5 ksi
ASTM D790
Ineos Nova 1511 High Heat Crystal Polystyrene  (discontinued **)
High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical..
Flexural Modulus 3.037 GPa
440.5 ksi
ASTM D790
Ineos Nova 2100 General Purpose Crystal Polystyrene  (discontinued **)
Relative high heat resistance, Improved crack resistance, Good strengthApplications: Foam extrusion, Biaxially oriented sheet, Thermoforming applications, Molded packagingExposure to gamma radiation..
Flexural Modulus 3.037 GPa
440.5 ksi
ASTM D790
Ineos Nova 3601 General Purpose Crystal Polystyrene  (discontinued **)
Easy flow for high productivity, excellent post molding scuff resistanceApplications: Medical, LabwareExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phys..
Flexural Modulus 3.037 GPa
440.5 ksi
ASTM D790
Ineos Nova 1300 High Heat Crystal Polystyrene
High heat resistance, High strength, Good processing characteristics, USP Class ViApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation..
Flexural Modulus 3.037 GPa
440.5 ksi
ASTM D790
Ineos Nova 1510 High Heat Crystal Polystyrene
High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical..
Flexural Modulus 3.037 GPa
440.5 ksi
ASTM D790
Ineos Nova 1301 High Heat Crystal Polystyrene
High heat resistance, High strength, Good processing characteristics, USP Class VIApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation..