Mechanical Properties Metric English Comments
Flexural Modulus 2.91 GPa
422 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 6935 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.91 GPa
422 ksi
ASTM D790
PolyOne Geon™ Vinyl Dry Blend E7130 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.91 GPa
422 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Lubricomp KZL34 POM
LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas..
Flexural Modulus 2.91 GPa
422 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL LTA1350 PPE+PS
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Flexural Modulus 2.91 GPa
422 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Flexural Modulus 2.91 GPa
422 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL LTA5020 PPE+PS
Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Flexural Modulus 2.91 GPa
422 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66
LNP* LUBRICOMP* RI001 is a compound based on Nylon 66 resin containing 2% Silicone. Added feature of this grade is: Wear Resistant.
Flexural Modulus 2.91 GPa
422 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..