Polymer Property : Flexural Modulus = 420.5 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.899 GPa
420.5 ksi
ASTM D790
Nylene® Mach 6 , Fast Cycle Nylon 6
Description: Nylene® Mach is a fast cycle, high speed, high flow nylon 6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resourc..
Flexural Modulus 2.899 GPa
420.5 ksi
ASTM D790
Ravago Manufacturing Americas Enviramid™ N1300HL BK/UV2 Post Consumer Recycle Nylon 66
Heat Stabilized, Lubricated, UV Stabilized, Black and made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago.
Flexural Modulus 2.899 GPa
420.5 ksi
ASTM D790
Ravago Manufacturing Americas Enviramid™ N1300HL Nylon 66
Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
Flexural Modulus 2.899 GPa
420.5 ksi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0437G10M20CL Glass/Mineral Reinforced Coupled
Flexural Modulus 2.899 GPa
420.5 ksi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0334T30L Talc Reinforced
Flexural Modulus 2.899 GPa
420.5 ksi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0336T30L Talc Reinforced
Flexural Modulus 2.899 GPa
420.5 ksi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0436G20CL Glass Reinforced