Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 28.9 GPa | 4190 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP VERTON E9007E PEI LNP* VERTON* E9007E is a compound based on Polyetherimide (PEI) containing 35% Long Carbon Fiber. Added features of this grade include: Structural, High Temperature |