Polymer Property : Flexural Modulus = 405 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.79 GPa
405 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers MS 130HF Styrene Methyl Methacrylate Terpolymer
Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc.
Flexural Modulus 2.79 GPa
405 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics GELOY FXW749SK ASA
Sparkle VisualFx ASA Resin - Weatherable
Flexural Modulus 2.79 GPa
405 ksi
ASTM D790
Quadrant EPP Quadrant Nylon 612
Flexural Modulus 2.79 GPa
405 ksi
6.4 mm; ASTM D790
SABIC Innovative Plastics Lexan® FL903 PC
Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance, excellent impact, flexural strength/rigidity. UV-stabilized.
Flexural Modulus 2.79 GPa
405 ksi
6.4 mm; ASTM D790
SABIC Innovative Plastics Lexan® FL900 PC (Asia Pacific)
Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance excellent impact, flexural strength/rigidity. UL94 V-1 at .157"" (3.99 mm).
Flexural Modulus 2.79 GPa
405 ksi
ASTM D790
Ravago Manufacturing Americas Hylon® N2000HL Nylon 6 (DAM)
Information provided by Ravago.
Flexural Modulus 2.79 GPa
405 ksi
ASTM D790
PolyOne Geon™ Vinyl Fittings 210(HS) Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.79 GPa
405 ksi
6.4 mm; ASTM D790
SABIC Innovative Plastics Lexan® FL900 PC
Lexan* resin FL900 is a Br- & Cl-free flame retardant grade that can be foamed for weight reductions. UL-94 V1 listed at 3.9mm together with good stiffness, heat, creep and impact performance make i..
Flexural Modulus 2.79 GPa

@Thickness 3.20 mm
405 ksi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical HT700 ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Flexural Modulus 2.79 GPa

@Thickness 3.20 mm
405 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY SG5009F PC/ABS
Description: Injection Molding, PC/ABS, High Gloss, Scratch Resistance, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC & Monitor housing)CAS: 103598-77-2 and 181028-79-5Information prov..
Flexural Modulus 2.79 GPa

@Thickness 3.20 mm
405 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio..
Flexural Modulus 2.79 GPa

@Thickness 3.20 mm
405 ksi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical XG569C MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
Flexural Modulus 2.79 GPa
405 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp OP005XXC PPS
LNP LUBRICOMP* OP005XXC is a compound based on Polyphenylene Sulfide resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-..
Flexural Modulus 2.79 GPa
405 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OP005XXC PPS - LINEAR
LNP LUBRICOMP* OP005XXC is a compound based on PPS - Linear resin containing 25% PTFE/Silicone. Added features of this material include: Wear Resistant.
Flexural Modulus 2.79 GPa
405 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OP005XXC PPS (Asia Pacific)
LNP* LUBRICOMP* OP005XXC is a compound based on Polyphenylene Sulfide resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Flexural Modulus 2.79 GPa
405 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66
LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Flexural Modulus 2.79 GPa
405 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66 (Asia Pacific)
LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Flexural Modulus 2.79 GPa
405 ksi
ASTM D790
Samyang Tramid® 210P Polyamide, High Productivity
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210P is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT..
Flexural Modulus 2.79 GPa
405 ksi
ASTM D790
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced
Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by..
Flexural Modulus 2.79 GPa
405 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC
LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Flexural Modulus 2.79 GPa
405 ksi
ASTM D-790
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding
Georgia Gulf ProTherm® 4526 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high res..
Flexural Modulus 2.79 GPa
405 ksi
ASTM D790
Asahi Kasei Tenac®-C EF750 Acetal Copolymer, Antistat  (discontinued **)
Antistatic grade containing special carbon black.Applications: Parts requiring antistatic properties.This product is not a part of the standard product line dated 2003.
Flexural Modulus 2.79 GPa
405 ksi
Abatron AboCast 50-11/AboCure 50-12 Epoxy
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/13.5 ratio. Pot life: 500 g, 36 min. at 25°C (77°F). Exothermic Peak 265°C (510°F). Hardens in 2-24 hou..