Mechanical Properties Metric English Comments
Flexural Modulus 2.78 GPa
403 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Geloy EXGY30CP ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.78 GPa
403 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Geloy FXTW30PE ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.78 GPa
403 ksi
ASTM D790
PolyOne Geon™ Vinyl Dry Blend E7000 Polyvinyl Chloride, Rigid (PVC, Rigid)
60 degree gloss comparisons: Geon E7000 is 47-49;Geon E7456 is 40-49;Geon E7130 is 38-43;Geon E7370 is 26-31Information provided by PolyOne
Flexural Modulus 2.78 GPa
403 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Geloy FXTW30CP ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.78 GPa
403 ksi
ISO 178
Polyplastics Duranex® 209A Polybutylene Terephthalate (PBT), Low friction, Low wear
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 2.78 GPa
403 ksi
2.8mm/min; ASTM D790
Asia International Enterprise (Hong Kong) 3010FW Polybutylene terephthalate
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Flexural Modulus 2.78 GPa
403 ksi
2.0 in/min; ASTM D790
LTL Color Compounds ColorFast® NY1 Nylon 6
Injection molding nylon 6, with or without lubeAll information provided by LTL Color Compounders, Inc.
Copyright © lookpolymers.com All Rights Reserved