Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.24 - 2.76 GPa | 180 - 400 ksi | Average value: 1.99 GPa Grade Count:18 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Flexural Modulus | 2.07 - 2.76 GPa | 300 - 400 ksi | ASTM D790 |
Alcoa KAMA 5100 CPET
(discontinued **) CapabilitiesGauge: .020" to .040" (508 to 106µm)Width: 20" to 52" (508 to 1321mm)Core size: 3" or 6"Roll O.D.: 29" standard, available up to 40"Silicone coating availableAvailable in natural blackP.. |
|||
Flexural Modulus | 1.38 - 2.76 GPa | 200 - 400 ksi | ASTM D790 |
Alcoa KAMA 3000 High Impact Polystyrene (HIPS)
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Flexural Modulus | 1.38 - 2.76 GPa | 200 - 400 ksi | ASTM D790 |
Alcoa KAMA 3210 Hi-Gloss Coextruded High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Flexural Modulus | 1.37 - 2.76 GPa | 199 - 400 ksi | Average value: 2.09 GPa Grade Count:36 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Flexural Modulus | 2.07 - 2.76 GPa | 300 - 400 ksi | Average value: 2.40 GPa Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Flexural Modulus | 1.38 - 2.76 GPa | 200 - 400 ksi | ASTM D790 |
Alcoa KAMA 3200 Prime High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone trea.. |