Polymer Property : Flexural Modulus = 4.93 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0340 GPa

@Temperature 49.0 °C
4.93 ksi

@Temperature 120 °F
ASTM D790
DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.0340 GPa
4.93 ksi
1% Secant, ASTM D790
ExxonMobil Escorene® LD-724 High EVA Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty compounding applications. Outstanding heat sealability along with excellent strength properties ..