Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.80 GPa | 696 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 15 LS Polyamide 6, 15% Glass Fiber, UV Stabilization FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools... |
|||
Flexural Modulus | 4.80 GPa @Temperature 90.0 °C |
696 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT Description: Nilitop BT G6 is a general purpose, 30% glass fiber reinforced PBT. This product has good overall mechanical performance, low moisture absorption and excellent UV resistance. It is used.. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP BX05030 SAN (Europe-Africa-Middle East) LNP* Lubricomp* BX05030 is a compound based on Styrene Acrylonitrile resin containing Mineral, Graphite. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ASTM D790 |
Custom Resins Vexel™ 5100 RD PBT; 15% Glass Filled
(discontinued **) Improved Surface. Property data for dry as molded samples.Data provided by the manufacturer |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ASTM D790 |
Resinoid 2205 Phenolic Molding, Cellulose Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | |
Plastcom SLOVAMID 6 T 20 PA6, 20% mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased modulus in tension - strength of the material. PA matrix reduction. Application eg. for tools, fi.. |
|||
Flexural Modulus | 4.80 GPa @Temperature 23.0 °C |
696 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH GF8030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | conditioned, 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 130 H3.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, glass fiber, injection molding, impact modified, heat-aged stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 226F3 Nylon 6.6, 15% Glass Fiber SAXAMID 226F3 is a polyamide 6.6 injection-molding-grade reinforced with 15% glass fibers. This grade is suitable for applications requiring high strength and very good flow properties during proces.. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ASTM D790 |
PlastxWorld Veroplas PB3150 Nylon 66 15% glass filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ISO 178-93 |
Wellman Wellamid® GS40-66 22L-Bk1 40% Glass Sphere Filled Nylon 66 Description: Glass Sphere Filled Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ASTM-D790 |
Polyram RamSter PF320G2 PBT, 10% Glass Fiber, Flame Retardant 10% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ASTM-D790 |
Polyram RamSter PF320G3 PBT, 15% Glass Fiber, Flame Retardant 15% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ASTM-D790 |
Polyram PlusTek PB320G3 Nylon 6, 15% Glass Fiber, Flame Retardant 15% glass-fiber reinforced, flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ISO 178 |
Polyram RamSter PF321G2 PBT, 10% Glass Fiber, Flame Retardant 10% Glass fiber reinforced, flame retardant PBT for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ISO 178 |
Polyram RamTough PZ305G4 Polycarbonate, 20% Glass Fiber 20% glass fiber reinforced polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000/58 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Impact Modified Until -40°C, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal (POM)
(Unverified Data**) 10% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength stiffness and high deflection temperatu.. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ASTM D790 |
E-Polymers TEKAMID® TB120G15 , 15% Glass Fiber Reinforced PA6, DAM 15% Glass Fiber reinforced, Good surface Information provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | Transverse direction; ISO 178 |
Azdel Plus U421-B01 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421-B01 is a glass mat thermoplastic laminate based upon a combination of random oriented continuous fiber mat and oriented fiber mat contained within a polypropylene resin matrix. This co.. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ASTM D790 |
Adell AR-13 Nylon 66, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ASTM D790 |
Adell AR-33 Nylon 66, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ISO 178 |
BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Dry) Description: Ultramid SEGM35 H1 BK6259 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compar.. |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ASTM D790 |
Ashley Polymers Ashlene® 73M Nylon 6, Mineral Reinforced A mineral reinforced Nylon 6 with improved impact, excellent dimensional stability and heat resistance.Data provided by the manufacturer |
|||
Flexural Modulus | 4.80 GPa | 696 ksi | ASTM-D790 |
Polyram PlusTek PB312J6 Nylon 6, 30% Glass Fiber 30% glass-fiber reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |