Mechanical Properties Metric English Comments
Flexural Modulus 0.0310 GPa
4.50 ksi
1% Secant, ASTM D790
ExxonMobil Escorene® LD-740 High EVA Film and Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr..
Flexural Modulus 0.0310 GPa

@Temperature 49.0 °C
4.50 ksi

@Temperature 120 °F
ASTM D790
DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.0310 GPa
4.50 ksi
ASTM D790
Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Flexural Modulus 0.0310 GPa
4.50 ksi
ASTM D790
Lubrizol Estane® ALR PC95A Thermoplastic Polyurethane
Type: Estane® ALR PC95A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi..
Flexural Modulus 0.0310 GPa
4.50 ksi
1% secant; ASTM D790
ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin
Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be ..
Flexural Modulus 0.0310 GPa
4.50 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 A
Dow FLEXOMER™ GERS-1088 NT Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ GERS-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to..