Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Omni Plastics OmniTuff™ HPP GRMF30 Homopolymer Polypropylene Glass/Mineral Filled
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Niche Polymer PPHG20BK Homopolymer PP, 20% Glass Fiber Filled
Information provided by Niche Polymer
Flexural Modulus 4.34 GPa

@Temperature 22.8 °C
630 ksi

@Temperature 73.0 °F
ASTM D790
Quadrant EPP KETRON® MD PEEK, A Metal-Detectable Polyetheretherketone
Flexural Modulus 4.34 GPa
629 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
PolyOne Edgetek® PS-25MN/000 Polybutylene Terephthalate (PBT), Mineral Filled  (discontinued **)
Description/Features:Mineral FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 4.34 GPa
630 ksi
2.0 in/min; ASTM D790
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded
13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc.
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Techmer ES Electrablend® PA6/6 C BK
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Techmer ES Electrablend® PA6/PC
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive Appearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Techmer ES Statiblend® PA6 02012
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveUL File Number: E157318TPCI# 1038102Information provided by TP Composites, Inc.
Flexural Modulus 4.34 GPa
629 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS
LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Flexural Modulus 4.34 GPa
629 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Flexural Modulus 4.34 GPa
629 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF002SXS PA 66
LNP* THERMOCOMP* RF002SXS is a compound based on Nylon 66 resin contaning 10% Glass Fiber. Characteristcs of this grade are: Heat Stabilized.
Flexural Modulus 4.34 GPa
629 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOTUF RF002I PA 66
LNP THERMOTUF* RF002I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Flexural Modulus 4.34 GPa
629 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOTUF RF002I PA 66 (Asia Pacific)
LNP* THERMOTUF* RF002I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Techmer ES Electrablend® PA6 C BK
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 4.34 GPa
629 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP
LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Ensinger Tecapeek® XP-95 Compression Molded PEEK Compound, 15% PTFE Filled
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Clariant Renol PA113G13X050 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Improved Ductility
Data provided by Clariant Masterbatches
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Asahi Kasei Thermylene® P-25FG-3809 25% Glass Fiber Reinforced
Information provided by Asahi Thermofil
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Asahi Kasei Thermylene® P6-30FG-0708 30% Glass Fiber Reinforced, High Impact
Information provided by Asahi Thermofil
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
PolyOne Edgetek® PI-20GM/000 L Polyetherimide (PEI), Glass Filled  (discontinued **)
Description/Features:Milled Glass Fiber ReinforcedHigh FlowPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Chase Plastics CP Pryme® N310GL (DAM) Nylon 6 (Utility Grade), 10% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.