Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.26 GPa | 618 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp DFP22H PC LNP* Lubricomp* DFP22H is a compound based on Polycarbonate containing Glass Fiber and PTFE. Characteristics of this grade are: Internally Lubricated and Healthcare.This data was supplied by SABIC.. |
|||
Flexural Modulus | 4.26 GPa | 618 ksi | ISO 178 |
Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix AZDEL® C327-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |