Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0286 GPa | 4.15 ksi | ISO 178 |
Multibase TPSiV® 4100-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr.. |