Polymer Property : Flexural Modulus = 4.08 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.08 GPa
592 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid)
Physical properties based on Geon L6607 white 1363Information provided by PolyOne
Flexural Modulus 4.08 GPa
592 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP CBL36XXC PS (Asia Pacific)
LNP* Lubricomp* CBL36XXC is a compound based on Polystyrene resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 4.08 GPa
592 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Lubricomp DFP22 PC
LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer..
Flexural Modulus 4.08 GPa
592 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP CBL36XXC PS
LNP* LUBRICOMP* CBL36XXC is a compound based on Polystyrene resin containing 30% Glass Bead and 15% PTFE. Added features of this material include: Wear Resistant.
Flexural Modulus 4.08 GPa
592 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6 (Asia Pacific)
LNP* Stat-loy* PF303 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Antistat.