Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0276 GPa
4.00 ksi
Density 3 pcf
NOVA Chemicals Dylite® F271TN Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..
Flexural Modulus 0.0276 GPa
4.00 ksi
Density 3 pcf
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..
Flexural Modulus 0.0276 - 1.21 GPa
4.00 - 175 ksi
Average value: 0.223 GPa Grade Count:28
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Flexural Modulus 0.0276 GPa
4.00 ksi
ASTM D790
Multibase Multi-Flex® D 2010 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F..
Flexural Modulus 0.0276 GPa
4.00 ksi
1% secant; ASTM D790
ExxonMobil Escorene® AD2528 Adhesive Application Resin
Escorene Ultra AD 2528 is a very high flow rate, 27.6% Vinyl Acetate, copolymer, which is useful in formulating hot melt adhesives.Availability: Latin America, North America and South America Additi..