Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.488 GPa | 360.9 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 2100 P Compounding Grade Powder Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.488 GPa | 360.9 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3500 HF Injection Molding Grade, High Flow, Medium Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |