Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.42 GPa | 351 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M3890 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® FR30U ABS Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific) Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 1.3 mm/min; ASTM D790 |
Lavergne VYPET PBT 6300 BK PBT Unreinforced, Impact Modified Vypet PBT 6300 BK is an unreinforced PBT injection molding compound offering excellent dimensional stability, chemical resistance, low moisture absorption and good electrical properties.Features: Hi.. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific) NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific) LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific) LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL HN731A PPE+PS PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine.. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific) Low odor grade for IC tray application |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL 731S PPE+PS (Asia Pacific) High heat PPO/HIPS alloy suitable for use in some potable water applications. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 2mm/min; ASTM D790 |
Denka TH-21 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Flexural Modulus | 2.42 GPa | 351 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |