Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.206 GPa
320.0 ksi
ASTM D790
Stratasys® Polyphenylsulfone
PPSF/PPSU (polyphenylsulfone) material has the greatest strength, heat and chemical resistance of all Stratasys materials - ideal for aerospace, automotive and medical applications. Stratasys FDM (F..
Flexural Modulus 2.206 GPa
320.0 ksi
ASTM D790
Ineos Nova 5190 High Impact Polystyrene  (discontinued **)
Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C ..
Flexural Modulus 2.206 GPa
320.0 ksi
ASTM D790
Proto3000 PPSF Fused Deposition Modeling Polymer
Description: PPSF/PPSU (polyphenylsulfone) material has the greatest heat and chemical resistance of all Fortus materials - ideal for aerospace, automotive and medical applications. PPSF parts manuf..
Copyright © lookpolymers.com All Rights Reserved