Mechanical Properties Metric English Comments
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120 Non-Reinforced, Injection Molding Grade Zinc Ionomer
DescriptionFormion® FI 120 is a non-reinforced, transparent, injection molding grade Zinc Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and lo..
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120 Non-Reinforced, Injection Molding Grade Zinc Ionomer
DescriptionFormion® FI 120 is a non-reinforced, transparent, injection molding grade Zinc Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and lo..
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120 Non-Reinforced, Injection Molding Grade Zinc Ionomer
DescriptionFormion® FI 120 is a non-reinforced, transparent, injection molding grade Zinc Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and lo..
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120 Non-Reinforced, Injection Molding Grade Zinc Ionomer
DescriptionFormion® FI 120 is a non-reinforced, transparent, injection molding grade Zinc Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and lo..
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120 Non-Reinforced, Injection Molding Grade Zinc Ionomer
DescriptionFormion® FI 120 is a non-reinforced, transparent, injection molding grade Zinc Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and lo..
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap..
Flexural Modulus 0.227 GPa
32.9 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 120 Non-Reinforced, Injection Molding Grade Zinc Ionomer
DescriptionFormion® FI 120 is a non-reinforced, transparent, injection molding grade Zinc Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and lo..
Copyright © lookpolymers.com All Rights Reserved